| Nonaqueous sol–gel synthesis of anatase nanoparticles and their electrophoretic deposition in porous alumina
Frantz, C., Lauria, A., Manzano, C. V., Guerra-Nuñez, C., Niederberger, M., Storrer, C., … Philippe, L. (2017). Nonaqueous sol–gel synthesis of anatase nanoparticles and their electrophoretic deposition in porous alumina. Langmuir, 33(43), 12404-12418. https://doi.org/10.1021/acs.langmuir.7b02103 |
| Micromechanics of amorphous metal/polymer hybrid structures with 3D cellular architectures: size effects, buckling behavior, and energy absorption capability
Mieszala, M., Hasegawa, M., Guillonneau, G., Bauer, J., Raghavan, R., Frantz, C., … Philippe, L. (2017). Micromechanics of amorphous metal/polymer hybrid structures with 3D cellular architectures: size effects, buckling behavior, and energy absorption capability. Small, 13(8), 1602514 (13 pp.). https://doi.org/10.1002/smll.201602514 |
| Electrodeposition of Lead telluride thin films and nanowires
Frantz, C., Zhang, Y., Michler, J., & Philippe, L. (2016). Electrodeposition of Lead telluride thin films and nanowires. Presented at the The 67 th Annual Meeting of the International Society of Electrochemistry. The Hague, The Netherlands. |
| On the growth mechanism of electrodeposited PbTe dendrites
Frantz, C., Zhang, Y., Michler, J., & Philippe, L. (2016). On the growth mechanism of electrodeposited PbTe dendrites. CrystEngComm, 18(13), 2319-2326. https://doi.org/10.1039/C6CE00107F |
| Electrodeposition of PbTe thin films: electrochemical behavior and effect of reverse pulse potential
Frantz, C., Vichery, C., Michler, J., & Philippe, L. (2015). Electrodeposition of PbTe thin films: electrochemical behavior and effect of reverse pulse potential. Electrochimica Acta, 173, 490-496. https://doi.org/10.1016/j.electacta.2015.05.045 |
| Pulse electrodeposition of adherent nickel coatings onto anodized aluminium surfaces
Frantz, C., Vichery, C., Zechner, J., Frey, D., Bürki, G., Cebeci, H., … Philippe, L. (2015). Pulse electrodeposition of adherent nickel coatings onto anodized aluminium surfaces. Applied Surface Science, 330, 39-47. https://doi.org/10.1016/j.apsusc.2014.12.091 |
| Electrodeposition and characterization of FeCrNi stainless steel alloy
Hasegawa, M., Tournoud, Z., Guillonneau, G., Zhang, Y., Frantz, C., Niedeberger, C., … Philippe, L. (2015). Electrodeposition and characterization of FeCrNi stainless steel alloy. Presented at the E-MRS 2015 spring meeting. Lille, FR. |
| Electrodeposition of lead telluride thin films and nanowires
Frantz, C., Vichery, C., Michler, J., & Philippe, L. (2014). Electrodeposition of lead telluride thin films and nanowires. Presented at the 40th international conference on micro and nano engineering (MNE 2014). Lausanne, Switzerland. |
| The electrodeposition of FeCrNi stainless steel: microstructural changes induced by anode reactions
Hasegawa, M., Yoon, S., Guillonneau, G., Zhang, Y., Frantz, C., Niederberger, C., … Philippe, L. (2014). The electrodeposition of FeCrNi stainless steel: microstructural changes induced by anode reactions. Physical Chemistry Chemical Physics, 16(47), 26375-26384. https://doi.org/10.1039/C4CP03744H |
| Stabilization mechanism of electrodeposited silicon thin films
Vichery, C., Le Nader, V., Frantz, C., Zhang, Y., Michler, J., & Philippe, L. (2014). Stabilization mechanism of electrodeposited silicon thin films. Physical Chemistry Chemical Physics, 16(40), 22222-22228. https://doi.org/10.1039/C4CP02797C |