On the investigation of quasi-static crack resistance of thermoplastic tape layered composites with multiple delaminations: approaches for quantification
Khudiakova, A., Brunner, A. J., Wolfahrt, M., Wettemann, T., Godec, D., & Pinter, G. (2021). On the investigation of quasi-static crack resistance of thermoplastic tape layered composites with multiple delaminations: approaches for quantification. Composites Part A: Applied Science and Manufacturing, 149, 106484 (10 pp.). https://doi.org/10.1016/j.compositesa.2021.106484
New insights into osteointegration and delamination from a multidisciplinary investigation of a failed hydroxyapatite-coated hip joint replacement
Schönweger, F., Sprecher, C. M., Milz, S., Dommann-Scherrer, C., Meier, C., Dommann, A., … Wahl, P. (2020). New insights into osteointegration and delamination from a multidisciplinary investigation of a failed hydroxyapatite-coated hip joint replacement. Materials, 13(21), 4713 (17 pp.). https://doi.org/10.3390/ma13214713
Fracture mechanics and oxygen gas barrier properties of Al<sub>2</sub>O<sub>3</sub>/ZnO nanolaminates on PET deposited by atomic layer deposition
Chawla, V., Ruoho, M., Weber, M., Chaaya, A. A., Taylor, A. A., Charmette, C., … Utke, I. (2019). Fracture mechanics and oxygen gas barrier properties of Al2O3/ZnO nanolaminates on PET deposited by atomic layer deposition. Nanomaterials, 9(1), 88 (17 pp.). https://doi.org/10.3390/nano9010088
Thoughts on the scatter seen in cyclic Mode I fatigue delamination growth in DCB tests
Mujtaba, A., Stelzer, S., Brunner, A. J., & Jones, R. (2017). Thoughts on the scatter seen in cyclic Mode I fatigue delamination growth in DCB tests. Composite Structures, 160, 1329-1338. https://doi.org/10.1016/j.compstruct.2016.11.002
Analysis of lignin degradation on wood surfaces to create a UV-protecting cellulose rich layer
Volkmer, T., Noël, M., Arnold, M., & Strautmann, J. (2016). Analysis of lignin degradation on wood surfaces to create a UV-protecting cellulose rich layer. International Wood Products Journal, 7(3), 156-164. https://doi.org/10.1080/20426445.2016.1200826
Thoughts on accounting for the scatter seen in delamination growth
Jones, R., Mujtab, A., Kinloch, T. J., Brunner, A. J., & Stelzer, S. (2015). Thoughts on accounting for the scatter seen in delamination growth. In AIAC16: 16th Australian international aerospace congress (pp. 262-267).
Mode I delamination fatigue crack growth in unidirectional fiber reinforced composites: results from ESIS TC4 round-robins
Stelzer, S., Brunner, A. J., Argüelles, A., Murphy, N., Cano, G. M., & Pinter, G. (2014). Mode I delamination fatigue crack growth in unidirectional fiber reinforced composites: results from ESIS TC4 round-robins. Engineering Fracture Mechanics, 116, 92-107. https://doi.org/10.1016/j.engfracmech.2013.12.002
An overview on diamond-like carbon coatings in medical applications
Hauert, R., Thorwarth, K., & Thorwarth, G. (2013). An overview on diamond-like carbon coatings in medical applications. Surface and Coatings Technology, 233, 119-130. https://doi.org/10.1016/j.surfcoat.2013.04.015
Failure modes of PVD coatings in molten Al-alloy contact
Lorusso, M., Ugues, D., Oliva, C., & Ghisleni, R. (2013). Failure modes of PVD coatings in molten Al-alloy contact. Acta Metallurgica Slovaca, 19(1), 30-42. https://doi.org/10.12776/ams.v19i1.84
Delamination detection in a 90-year-old glulam block with scanning dry point-contact ultrasound
Neuenschwander, J., Sanabria, S. J., Schuetz, P., Widmann, R., & Vogel, M. (2013). Delamination detection in a 90-year-old glulam block with scanning dry point-contact ultrasound. Holzforschung, 67(8), 949-957. https://doi.org/10.1515/hf-2012-0202
Retrospective lifetime estimation of failed and explanted diamond-like carbon coated hip joint balls
Hauert, R., Falub, C. V., Thorwarth, G., Thorwarth, K., Affolter, C., Stiefel, M., … Taeger, G. (2012). Retrospective lifetime estimation of failed and explanted diamond-like carbon coated hip joint balls. Acta Biomaterialia, 8(8), 3170-3176. https://doi.org/10.1016/j.actbio.2012.04.016
Modeling in-plane and out-of-plane displacement fields in pull-off tests on FRP strips
Martinelli, E., Czaderski, C., & Motavalli, M. (2011). Modeling in-plane and out-of-plane displacement fields in pull-off tests on FRP strips. Engineering Structures, 33(12), 3715-3725. https://doi.org/10.1016/j.engstruct.2011.08.008
Boron carbide/boron carbide-carbon nanofibers laminates with weak interfaces
Orlovskaya, N., Lugovy, M., Slyunyayev, V., Subbotin, V., Liang, F., Gou, J., … Graule, T. (2011). Boron carbide/boron carbide-carbon nanofibers laminates with weak interfaces. In N. Orlovskaya & M. Lugovy (Eds.), NATO Science for Peace and Security Series B. Boron rich solids: sensors, ultra high temperature ceramics, thermoelectrics, armor (pp. 1-11). https://doi.org/10.1007/978-90-481-9818-4_1
Air-coupled ultrasound inspection of glued laminated timber
Sanabria, S. J., Furrer, R., Neuenschwander, J., Niemz, P., & Sennhauser, U. (2011). Air-coupled ultrasound inspection of glued laminated timber. Holzforschung, 65(3), 377-387. https://doi.org/10.1515/HF.2011.050
Monitored assessment of structural integrity of multilayered glued laminated timber beams with air-coupled ultrasound and contact ultrasound imaging
Sanabria, S. J., Furrer, R., Neuenschwander, J., Niemz, P., & Sennhauser, U. (2011). Monitored assessment of structural integrity of multilayered glued laminated timber beams with air-coupled ultrasound and contact ultrasound imaging. In F. Divos (Ed.), 17th international nondestructive testing and evaluation of wood symposium (pp. 359-366). University of West Hungary.
Influence of wood properties and bonding parameters on bond durability of European Beech (<I>Fagus sylvatica</I> L.) glulams
Ohnesorge, D., Richter, K., & Becker, G. (2010). Influence of wood properties and bonding parameters on bond durability of European Beech (Fagus sylvatica L.) glulams. Annals of Forest Science, 67(6), 601 (10 pp.). https://doi.org/10.1051/forest/2010002
Structural health monitoring of glued laminated timber with a novel air-coupled ultrasound method
Sanabria, S. J., Neuenschwander, J., Niemz, P., & Sennhauser, U. (2010). Structural health monitoring of glued laminated timber with a novel air-coupled ultrasound method (p. (10 pp.). Presented at the 11th world conference on timber engineering (WCTE 2010). .
Fatigue delamination behaviour of unidirectional carbon fibre/epoxy laminates reinforced by Z-Fiber<SUP>®</SUP> pinning
Cartié, D. D. R., Laffaille, J. M., Partridge, I. K., & Brunner, A. J. (2009). Fatigue delamination behaviour of unidirectional carbon fibre/epoxy laminates reinforced by Z-Fiber® pinning. Engineering Fracture Mechanics, 76(18), 2834-2845. https://doi.org/10.1016/j.engfracmech.2009.07.018
Hydroxymethylated resorcinol (HMR) and novolak-based HMR (n-HMR) primers to enhance bond durability of <I>Eucalyptus globulus</I> Glulams
López-Suevos, F., & Richter, K. (2009). Hydroxymethylated resorcinol (HMR) and novolak-based HMR (n-HMR) primers to enhance bond durability of Eucalyptus globulus Glulams. Journal of Adhesion Science and Technology, 23(15), 1925-1937. https://doi.org/10.1163/016942409X12508517390914
Adhesion behaviour of glued laminated timber from European Beech
Ohnesorge, D., Richter, K., Becker, G., & Aicher, S. (2008). Adhesion behaviour of glued laminated timber from European Beech (pp. 110-118). Presented at the Enhancing bondline performance – final conference of COST E34 bonding of timber. .