Deep-UV-enhanced approach for low-temperature solution processing of IZO transistors with high-<em>k</em> AlO<em><sub>x</sub></em>/YAlO<em><sub>x</sub></em> dielectric
Mancinelli, A., Bolat, S., Kim, J., Romanyuk, Y. E., & Briand, D. (2020). Deep-UV-enhanced approach for low-temperature solution processing of IZO transistors with high-k AlOx/YAlOx dielectric. ACS Applied Electronic Materials, 2(10), 3141-3151. https://doi.org/10.1021/acsaelm.0c00444
The interplay of shape and crystalline anisotropies in plasmonic semiconductor nanocrystals
Kim, J., Agrawal, A., Krieg, F., Bergerud, A., & Milliron, D. J. (2016). The interplay of shape and crystalline anisotropies in plasmonic semiconductor nanocrystals. Nano Letters, 16(6), 3879-3884. https://doi.org/10.1021/acs.nanolett.6b01390