Mechanical behavior of intragranular, nano-porous electrodeposited zinc oxide
Raghavan, R., Elias, J., Erni, R., Parlinska, M., Philippe, L., & Michler, J. (2015). Mechanical behavior of intragranular, nano-porous electrodeposited zinc oxide. Thin Solid Films, 578, 174-179. https://doi.org/10.1016/j.tsf.2015.02.017